Barium titanate thick films prepared by screen printing technique

ADD TO MY LIST
 
Author(s): Mirjana M. Vijatović | Jelena D. Bobić | Biljana D. Stojanović | Barbara Malič

Journal: Processing and Application of Ceramics
ISSN 1820-6131

Volume: 4;
Issue: 2;
Start page: 53;
Date: 2010;
VIEW PDF   PDF DOWNLOAD PDF   Download PDF Original page

Keywords: BaTiO3 | Thick film | Screen printing | Electrical properties

ABSTRACT
The barium titanate (BaTiO3) thick films were prepared by screen printing technique using powders obtained by soft chemical route, modified Pechini process. Three different barium titanate powders were prepared: i) pure, ii) doped with lanthanum and iii) doped with antimony. Pastes for screen printing were prepared using previously obtained powders. The thick films were deposited onto Al2O3 substrates and fired at 850°C together with electrode material (silver/palladium) in the moving belt furnace in the air atmosphere. Measurements of thickness and roughness of barium titanate thick films were performed. The electrical properties of thick films such as dielectric constant, dielectric losses, Curie temperature, hysteresis loop were reported. The influence of different factors on electrical properties values was analyzed.