ABSTRACT
The porous alumina as a plate catalytic support was prepared by anodization. Effects of hydration condition on the property of alumina supports were studied. The samples were characterized by XRD, SEM, BET and etc. to illustrate the Al2O3/Al forming mechanism. The results show that the best hydration temperature is 80¡䪠at which the amorphous alumina can be transformed into AlOOH, and become γ-Al2O3 after 500¡䟣alcination. Meanwhile, the monoliths catalytic carriers have a superior stability for crystalline structures in the steam atmosphere at high temperature.

Tango Rapperswil
Tango Rapperswil

     Save time & money - Smart Internet Solutions